ceria 33 - An Overview
SEM (Tescan Vega (LMU)) was used to look at the cross-sectional and surface morphology with the membranes of different NP loadings (Figure one and Figure S1). Membranes have been damaged in liquid nitrogen to fix the cross-sectional ends on the membranes along with a voltage of fifteen–twenty Kv at distinct magnifications was used with gold coati